I have a 84 atc 70 that the tank has started to rust. I dont really want to mess up my original tank. Does anyone do this professionally?
thanks
I have a 84 atc 70 that the tank has started to rust. I dont really want to mess up my original tank. Does anyone do this professionally?
thanks
its easy get some Kream the 3 part kit, a bucket and some good gloves ive done 3 tanks atc 70, atc 200x, and atc250r. and its super simple to do. for the atc 70 tank you will have enough kream to do like 3-4 tanks
83 250R![]()
91 CR125R![]()
redkote works great too, and i lot of people prefer it over kreeme here on the boards. Search for redkote or red kote and youll find tons of threads.
It can be bought on ebay also.
Mike
1986 Tri-z
1985 250r
1985 200s
1985 70[/SIZE]
I always used POR-15, always worked wonders for my trikes.
Rest in peace Rex Carlson
I use Red-Kote and do all my tanks myself. It really easy to use and the results have been super so far. It's easy enough that even a Caveman can do it. lmaoOriginally Posted by 2000ssm6
Howdy
hey... cavemen have feelings too ya know....![]()
I'm sorry, I didn't know they were still around!!. lmaoOriginally Posted by tyman
Howdy
Hey howdy i am somewhat near you and i am going to be picking up a 200s and 200x roller from your brother dale(when i find a truck to use, lol). Im pretty sure he said he has a tank i could get too but i dont know if it is rusty on the inside or nice on the inside. How much would you want to coat the inside of it if i needed you to? Thanks!
Craig
'86 200x
I normally charge $35 plus shipping cost ( if shipped ). Turn around time is about 1 week ( from the time I get it until I ship it ). The reason for the extra time is that I allow the tank to dry completely before I ship it out. The was mandated by UPS and USPS.
Howdy
Alright, if i end up getin it done, i will send ya a PM. Thanks Howdy!
Craig
'86 200x